Knowledge · Process & Formulation
Process & Formulation
What happens between the feed throat and the pelletizer: temperature profiles by material family, filler and masterbatch recipes, engineering plastics compounding, pelletizing choice, feeding accuracy and the kilograms you lose at start-up and grade change.
This page collects our floor notes on twin screw extruder process: how the line is laid out, the numbers we reference most, and the checks that prevent the usual startup problems.
- Masterbatch Carrier Selection: MFR, Compatibility & the One Rule
Masterbatch Carrier Selection: one rule covers 90% of carrier selection: use the same or a compatible resin as the customer's end polymer, with an MFR…
Process & formulation · 6 min read - MAH Grafting on PP/PE: Liquid Injection, Twin Vacuum & the 0.8–1.2% Target
MAH Grafting: maleic-anhydride grafting turns polyolefins into compatibilizers (PP-g-MAH, PE-g-MAH) by reacting MAH onto the chain in the melt — with…
Process & formulation · 6 min read - HFFR Cable Compound: Why Two-Stage Beats Single Screw
Halogen-free flame-retardant (HFFR) cable compounds carry 50–60% ATH/MH filler, and aluminum trihydrate starts releasing water above ~200°C.
Process & formulation · 6 min read - Flame Retardant Masterbatch: Formulation & Temperature Red Lines
Flame Retardant Masterbatch Formulation: halogen-free flame-retardant masterbatch concentrates 70–80% phosphorus-nitrogen FR package into a carrier — and the…
Process & formulation · 6 min read - Why the First Barrel Zone Runs at 80–120°C in Filler Masterbatch
First Zone Temperature: filler masterbatch temperature profiles deliberately start low — first zone 80–120°C, sometimes as low as 80°C on high-percentage…
Process & formulation · 6 min read - Filler Masterbatch Formulation Structure: The Four-Component Skeleton
Filler Masterbatch Formulation Structure: every filler masterbatch is the same four-part skeleton with different numbers: filler 70–85%, carrier 12–25%…
Process & formulation · 6 min read - Coupling Agent Activation: 0.8–1.5% Dosage at 110–120°C
Coupling Agent Activation: coupling agents are the cheapest component in a filler masterbatch and the one that decides whether the filler works.
Process & formulation · 6 min read - Color Masterbatch Formulation Guide: Pigment, Carrier & Dispersion
Color Masterbatch Formulation Guide: a color masterbatch is pigment 10–50% (organic 10–25%, inorganic 20–50%), carrier resin chosen to match the customer's…
Process & formulation · 6 min read - Carbon Black Masterbatch: Formulation Windows from Pipe to Food Grade
Carbon Black Masterbatch Formulation: carbon black masterbatch lives in a 35–42% pigment window for general grades, rises to 46–48% for pipe grades (with…
Process & formulation · 6 min read - 80% CaCO₃ Masterbatch Line: The Two-Stage Setup
A filler masterbatch above 80% CaCO₃ is the classic two-stage application: one co-rotating twin screw to melt, activate-load and disperse the mineral, one slo
Process & formulation · 6 min read - CaCO₃ Filler Masterbatch: Typical Formulation & Process Window
A production-credible CaCO₃ filler masterbatch runs 70–85% mineral, 12–25% carrier, 0.8–1.5% aluminate coupling agent and 3–5% PE-wax/stearate package.
Process & formulation · 6 min read - Antistatic & Conductive Masterbatch: Formulation and the CNT Dosing Problem
Conductive Masterbatch Formulation: antistatic masterbatch comes in two chemically opposite formats: migratory surface agents (GMS/ethoxylated amines, 15–25%…
Process & formulation · 6 min read - Antibacterial Masterbatch: Formulation & the 230°C Silver Line
Masterbatch Formulation: antibacterial masterbatch carries silver-ion zeolite or phosphate carrier actives at 5–20% concentration, and its defining…
Process & formulation · 6 min read - ABS Flame-Retardant Compound: Formulation & the Two-Dryer Rule
Flame Retardant Compound Formulation: aBS flame-retardant compounding is a twin-screw blending job with one non-obvious infrastructure demand: PC/ABS alloys…
Process & formulation · 7 min read - Silane Crosslinked PE–Rubber Compound: Processing and KTE-65B Line Configuration
Rubber-modified silane crosslinked PE on a KTE-65B: two-step grafting, 140–200 kg/h reference output, and when strand pelletizing stops working.
Process & formulation · 14 min read - Black Masterbatch: Why 40% Carbon Black Costs You 20-25% Output
Black masterbatch at 40% carbon black runs 20–25% below colour output on the same machine — dispersion, filtration and dispersant dosage set the gap.
Process & formulation · 5 min read - 80-90% CaCO3 Masterbatch: The Line Layout That Actually Runs It
Two-stage layout for 85-90% CaCO3 masterbatch: 350-600 kg/h on KTE/SE-65/150, 110-120C activation, bimetallic wear package and hot-face pelletising.
Process & formulation · 4 min read - PLA & Biodegradable Pelletizing: The 170-200°C Window
PLA pelletizing window 170-200C, drying to 0.05% moisture at 80C x 4h, mild screw work, air-cooling strand cutting, and the chain-extender route.
Process & formulation · 4 min read - Start-up Scrap on a Twin Screw Line: Measure It, Then Cut It
Typical startup scrap by machine size and L/D, the four design levers that reduce it, grade-change costs, and the contract clause that makes it enforceable.
Process & formulation · 6 min read - Why the Feeding System Sets the Throughput Ceiling
Why feeding throughput, not screw speed, sets the output ceiling: feeder accuracy by material, side-feed rules and the mass-balance math.
Process & formulation · 8 min read - Seven Pelletizing Methods Compared
Pelletizing methods compared — The pelletizer is chosen by the polymer, not by the budget. This table compares all seven methods we build on the criteria.
Process & formulation · 5 min read - Engineering Plastics Compounding: PA, PBT, PC and ABS
Engineering plastics compounding on a twin screw: drying, glass-fibre side feeding, screw design for PA, PBT, PC and ABS, and the temperature windows.
Process & formulation · 12 min read - Filler Masterbatch Line: Configuration, Formulation and Output
Filler masterbatch line reference: 75–90% CaCO3 or talc loading, screw configuration, feeder discipline, wear package and output by KTE model.
Process & formulation · 16 min read - Twin Screw Extruder Temperature Profile by Material
Twin screw extruder temperature profile by material: zone 1, melt peak, metering and die temperatures for 16 material families.
Process & formulation · 18 min read
FAQ
My formulation is not in these tables — what now?
Send 25–50 kg of polymer and additives. Every range on these pages is a measured reference, not a catalogue maximum; we replace the estimate with a measured number from a trial on your material.
Where does start-up scrap fit into process decisions?
Into the L/D decision and the pelletizing architecture. Both are fixed at order stage and set the floor for every start and grade change afterwards; the operating-cost page shows the arithmetic.
Other sections: Machines & Selection · Service & Operation · Extrusion lines by application · free line quotation
Bottom line. What happens between the feed throat and the pelletizer: temperature profiles by material family, filler and masterbatch recipes, engineering plastics compounding, pelletizing choice, feeding accuracy and the kilograms you lose at start-up and grade change. Use the references above to shortlist, then let the material decide: a 25–50 kg lab trial settles filler ceiling, pellet shape and output before you commit to a line.