Engineering Plastic Compounding

Home/Applications/Engineering Plastic Compounding Application · Engineering Plastics Engineering Plastic Compounding: PA, PC, PBT, ABS & Alloys Engineering plastics punish shortcuts in two places: drying (PA and PC want 120 °C for four hours, not 80 °C overnight) and fibre handling (side feed position decides how much of the fibre survives). A reference engineering plastic compounding […]

Glass Fiber Compounding: Protect Fiber Length

Home/Applications/Glass Fiber Compounding Application · Engineering Plastics Glass Fiber Compounding: Protect Fiber Length Glass fibre reinforcement is not about getting fibre in — it is about not breaking it on the way through. Screw geometry after the side feeder decides whether you keep 0.6 mm or 0.25 mm average length. A reference glass fiber compounding […]