Beranda/Aplikasi/Compounding Plastik Rekayasa

Aplikasi · Plastik Rekayasa

Compounding Plastik Rekayasa: PA, PC, PBT, ABS & Paduan

Plastik rekayasa menghukum jalan pintas di dua tempat: pengeringan (PA dan PC ingin 120 °C selama empat jam, bukan 80 °C semalam) dan penanganan serat (posisi side feeder menentukan berapa banyak serat yang selamat). Halaman referensi compounding plastik rekayasa dari Kerke.

Compounding Plastik Rekayasa — foto workshop 1, workshop Kerke, NanjingCompounding Plastik Rekayasa — foto workshop 1, workshop Kerke, Nanjing
Compounding Plastik Rekayasa — foto workshop 2, workshop Kerke, NanjingCompounding Plastik Rekayasa — foto workshop 2, workshop Kerke, Nanjing
Compounding Plastik Rekayasa — foto workshop 3, workshop Kerke, NanjingCompounding Plastik Rekayasa — foto workshop 3, workshop Kerke, Nanjing
Compounding Plastik Rekayasa — foto workshop 4, workshop Kerke, NanjingCompounding Plastik Rekayasa — foto workshop 4, workshop Kerke, Nanjing
Compounding Plastik Rekayasa — foto workshop 5, workshop Kerke, NanjingCompounding Plastik Rekayasa — foto workshop 5, workshop Kerke, Nanjing
Compounding Plastik Rekayasa — foto workshop 6, workshop Kerke, NanjingCompounding Plastik Rekayasa — foto workshop 6, workshop Kerke, Nanjing
Video berjalan — Compounding Plastik Rekayasa, workshop Kerke
Video berjalan — Compounding Plastik Rekayasa, workshop Kerke

Jawaban cepat

Compounding plastik rekayasa (PA, PBT, PC, ABS, PC/ABS, POM) berjalan pada ulir ganda torsi tinggi dengan L/D 40–48, feeding serat atau filler di hilir, devolatilisasi vakum, dan output 300–3,000 kg/h. Kepadatan torsi (T/A³ 8–12) lebih penting daripada daya motor untuk formulasi ini.

140–200 kg/hKTE-65D, diperkuat GF
2–4port side feed
120 °C × 4 jampengeringan PA / PC

Foto workshop dan video berjalan — diambil pada lini kami sendiri, bukan gambar stok.

Apa yang menetapkan batasnya

Resin dikeringkan, di-dosing, dan dilelehkan; serat kaca atau filler mineral ditambahkan di barrel 4–6; lelehan di-devolatilisasi di bawah vakum, difilter, dan dipelletizing underwater atau dengan strand.

Tabel 1. Parameter kunci lini compounding plastik rekayasa. Nilai referensi — konfirmasi lewat uji material.
ParameterNilai / rentang
PolimerPA6/PA66, PBT, PC, ABS, PC/ABS, POM
L/D40–48
Kelas torsiGearbox tipe D, T/A³ 8–12
HilirSide feeder, vakum 2 tahap, screen changer
Output (referensi)300–3,000 kg/h
ModelKTE-65D, KTE-75D, KTE-95D

Angka output lini compounding plastik rekayasa diukur pada material referensi yang dinyatakan di atas. Kandungan kaca dan viskositas polimer dasar menggeser output ±15% — itulah mengapa setiap penawaran yang kami terbitkan terikat pada laporan uji coba.

Alur proses, langkah demi langkah

  1. FeedingDosing Loss-in-weight polimer dan filler; side feeder atau injeksi cairan di mana formulasi membutuhkannya.
  2. Pelelehan dan disperseGeometri ulir dengan blok kneading 45°/90°; profil barrel ditentukan oleh polimer.
  3. DevolatilisasiVent vakum pada −0,06 sampai −0,09 MPa menghilangkan kelembapan dan volatil sebelum die.
  4. Penumpukan tekananThrottle or discharge section stabilises die pressure; a melt pump where gauge control matters.
  5. Pelletizing dan pengemasandie-face or strand pelletizing, see the pelletizing page; then centrifugal dryer, vibrating screen and bagging.

Konfigurasi peralatan

Tabel 2. Dari apa lini tersusun, dan mengapa tiap bagian dispesifikasi demikian.
TahapPeralatanMengapa pilihan ini
Mesin utamaExtruder Ulir Ganda SearahArsitektur mengikuti level pengisian dan tugas mixing, bukan tonase yang dibutuhkan.
Geometri ulirElemen modul bangunan, W6Mo5Cr4V2, liner bimetalPaket anti-usang untuk filler abrasif; blok mixing hanya di mana disperse menuntutnya.
FeedingLoss-in-weight feeder, side feeder bila diperlukanAkurasi resep: ±0.5% jangka pendek pada komponen tertimbang.
PelletizingSistem pelletizingDipilih berdasarkan polimer dan plafon filler — kontak air adalah kolom penentunya.
DownstreamCentrifugal dryer, vibrating screen, pengepakanFines di bawah 2% dan kelembapan di bawah spesifikasi proses hilir Anda.

Output per model

Tabel 3. Ulir ganda searah KTE — output referensi. Rentang lengkap di halaman mesin.
ModelDia. (mm)Kecepatan (rpm)Motor (kW)Torsi (N·m)Output (kg/h)
KTE-50B50.5500–60055–752×52580–200
KTE-50D50.5300–80075–902×860100–300
KTE-52B51.4500–60055–752×72080–200
KTE-52D51.4500–60075–1102×1050100–400
KTE-65B62.4500–60090–1102×860200–450
KTE-65D62.4300–800132–1602×1530350–600
KTE-75B71500–600132–1602×1530300–800
KTE-75D71300–800200–3152×2100500–1000
KTE-85B85500–600220–3152×2100550–1000
KTE-95B93500–600250–3152×3000800–1500
KTE-95D93500–800315–5002×48001000–2000
KTE-135B135500–600315–5002×48001500–3000
KTE-135D135500–800500–10002×78001500–4000

Tiga kesalahan paling mahal

1. Wet PA6

PA6 basah — kelembapan di atas 0.1% menghidrolisis polimer dan kekuatan impak runtuh.

2. Geseran tinggi setelah penambahan serat memutus seratnya; panjang serat di bawah 0.3 mm tidak memberikan penguatan.

Geseran tinggi setelah penambahan serat memutus seratnya; panjang serat di bawah 0.3 mm tidak memberikan penguatan.

3. Menyalin profil barrel PE ke PA atau PC

Menyalin profil barrel PE ke PA atau PC — PA menginginkan 240–270 °C, PC 260–290 °C ditambah pengeringan 4 jam pada 120 °C; profil generik diam-diam mengorbankan IV dan kekuatan impak.

FAQ

Gearbox B atau D untuk PA+30% GF?

Tipe D. Tipe B bekerja pada output berkurang dan umur sekrup lebih pendek; selisih harganya lebih kecil daripada kehilangan produktivitasnya.

Berapa L/D untuk PC/ABS?

40–44 tipikal; 48 jika Anda membutuhkan dua tahap vakum untuk grade VOC rendah.

Output berapa yang bisa kalian jamin untuk aplikasi ini?

Band referensinya adalah 300–3,000 kg/h, diukur pada material yang dinyatakan. Kami menawarkan angka terjamin hanya setelah uji coba pada material Anda sendiri, karena grade filler, bulk density, dan kelembapan menggeser output ±15%.

Bisakah kami menjalankan material kami sebelum memesan?

Ya — untuk lini compounding plastik rekayasa, kirim 25–50 kg compound-nya; laporannya menambahkan panjang serat residu dan riwayat suhu lelehan. Anda juga menerima pellet, video berjalan, serta suhu, kecepatan sekrup, dan setelan feeder yang kami pakai. Uji cobanya gratis; Anda menanggung fretenya.

Berapa waktu pengirimannya?

30–45 hari kerja untuk konfigurasi standar lini compounding plastik rekayasa, 45–70 untuk geometri sekrup kustom dan pekerjaan ODM — side feeder dan melt pump ditawarkan bersama lininya. Tegangan dan frekuensi dibangun untuk negara tujuan.

Dari mana angka-angka ini berasal

Parameter di halaman ini (lini compounding plastik rekayasa) diambil dari tabel parameter produk Kerke dan lembar data induk produk, serta disilangkan dengan rekaman commissioning lini compounding yang dibangun dalam beberapa musim terakhir. Formulasi dan jendela suhu adalah nilai tipikal industri untuk paduan rekayasa dan serat, bukan rekomendasi untuk compound spesifik Anda — setiap angka yang ditandai referensi harus dikonfirmasi lewat uji material sebelum menjadi angka kontraktual.

Direview oleh tim proses Kerke, Nanjing. Halaman diperbarui 6 November 2026.

Katakan material Anda — kami sebutkan lininya

Kirim 25–50 kg untuk uji coba lini compounding plastik rekayasa pada extruder laboratorium kami: pellet, video berjalan, dan laporan kapasitas kembali dalam 3–7 hari — laporannya menyertakan panjang serat residu di samping kapasitas.

Compounding plastik rekayasa — versi singkat

Catatan tentang compounding plastik rekayasa: angka-angka di atas adalah rentang referensi dari uji coba kami sendiri di Kerke, bukan janji katalog. Geometri sekrup, paket anti-usang, dan metode pelletizing ditentukan lebih dulu di bangku uji, jadi output yang Anda bandingkan adalah output yang Anda dapatkan. Jika grade Anda tidak ada di tabel, kirimkan — konfigurasi terdekat biasanya berupa pergantian set sekrup, bukan mesin yang berbeda.

Terkait di situs ini: Machine range: KTE-50B to 135D · Pelletizing methods compared · penawaran dan uji coba gratis · Wikipedia: Masterbatch