Beranda/Aplikasi/Compounding Serat Kaca

Aplikasi · Plastik Rekayasa

Compounding Serat Kaca: Lindungi Panjang Serat

Penguatan serat kaca bukan soal memasukkan serat — melainkan soal tidak memutuskannya di sepanjang jalannya. Geometri sekrup setelah side feeder menentukan apakah Anda mempertahankan panjang rata-rata 0,6 mm atau 0,25 mm. Halaman referensi compounding serat kaca dari Kerke.

Compounding Serat Kaca — foto workshop 1, workshop Kerke, NanjingCompounding Serat Kaca — foto workshop 1, workshop Kerke, Nanjing
Compounding Serat Kaca — foto workshop 2, workshop Kerke, NanjingCompounding Serat Kaca — foto workshop 2, workshop Kerke, Nanjing
Compounding Serat Kaca — foto workshop 3, workshop Kerke, NanjingCompounding Serat Kaca — foto workshop 3, workshop Kerke, Nanjing
Compounding Serat Kaca — foto workshop 4, workshop Kerke, NanjingCompounding Serat Kaca — foto workshop 4, workshop Kerke, Nanjing
Compounding Serat Kaca — foto workshop 5, workshop Kerke, NanjingCompounding Serat Kaca — foto workshop 5, workshop Kerke, Nanjing
Compounding Serat Kaca — foto workshop 6, workshop Kerke, NanjingCompounding Serat Kaca — foto workshop 6, workshop Kerke, Nanjing
Video berjalan — Compounding Serat Kaca, workshop Kerke
Video berjalan — Compounding Serat Kaca, workshop Kerke

Jawaban cepat

Compounding serat kaca berjalan pada 20–50% GF yang di-feed di hilir melalui side feeder ke ulir ganda torsi tinggi dengan L/D 44–52, barrel bimetal, dan sekrup yang dilindungi dari keausan. Output 300–2,500 kg/h; retensi panjang serat adalah metrik kualitas yang penting.

20–50%muatan serat kaca
L/D ≤ 44batas panjang sekrup
140–200 kg/hKTE-65D

Foto workshop dan video berjalan — diambil pada lini kami sendiri, bukan gambar stok.

Apa yang menetapkan batasnya

Resin meleleh di barrel-barrel pertama; roving ditarik masuk oleh side feeder dan dibasahi di zona geseran rendah; lelehan di-devolatilisasi dan dipelletizing menjadi strand dengan die yang dirancang untuk menghindari keselarasan serat.

Tabel 1. Parameter kunci lini compounding serat kaca. Nilai referensi — konfirmasi lewat uji material.
ParameterNilai / rentang
Kandungan GF20–50%
FeedingSide feeder di barrel 4–6
L/D44–52
Paket anti-usangBarrel bimetal, elemen ulir PM
Output (referensi)300–2,500 kg/h
ModelKTE-65D, KTE-75D, KTE-95D

Angka output lini compounding serat kaca diukur pada material referensi yang dinyatakan di atas. Kandungan kaca dan viskositas polimer dasar menggeser output ±15% — itulah mengapa setiap penawaran yang kami terbitkan terikat pada laporan uji coba.

Alur proses, langkah demi langkah

  1. FeedingDosing Loss-in-weight polimer dan filler; side feeder atau injeksi cairan di mana formulasi membutuhkannya.
  2. Pelelehan dan disperseGeometri ulir dengan blok kneading 45°/90°; profil barrel ditentukan oleh polimer.
  3. DevolatilisasiVent vakum pada −0,06 sampai −0,09 MPa menghilangkan kelembapan dan volatil sebelum die.
  4. Penumpukan tekananThrottle or discharge section stabilises die pressure; a melt pump where gauge control matters.
  5. Pelletizing dan pengemasandie-face or strand pelletizing, see the pelletizing page; then centrifugal dryer, vibrating screen and bagging.

Konfigurasi peralatan

Tabel 2. Dari apa lini tersusun, dan mengapa tiap bagian dispesifikasi demikian.
TahapPeralatanMengapa pilihan ini
Mesin utamaExtruder Ulir Ganda SearahArsitektur mengikuti level pengisian dan tugas mixing, bukan tonase yang dibutuhkan.
Geometri ulirElemen modul bangunan, W6Mo5Cr4V2, liner bimetalPaket anti-usang untuk filler abrasif; blok mixing hanya di mana disperse menuntutnya.
FeedingLoss-in-weight feeder, side feeder bila diperlukanAkurasi resep: ±0.5% jangka pendek pada komponen tertimbang.
PelletizingSistem pelletizingDipilih berdasarkan polimer dan plafon filler — kontak air adalah kolom penentunya.
DownstreamCentrifugal dryer, vibrating screen, pengepakanFines di bawah 2% dan kelembapan di bawah spesifikasi proses hilir Anda.

Output per model

Tabel 3. Ulir ganda searah KTE — output referensi. Rentang lengkap di halaman mesin.
ModelDia. (mm)Kecepatan (rpm)Motor (kW)Torsi (N·m)Output (kg/h)
KTE-50B50.5500–60055–752×52580–200
KTE-50D50.5300–80075–902×860100–300
KTE-52B51.4500–60055–752×72080–200
KTE-52D51.4500–60075–1102×1050100–400
KTE-65B62.4500–60090–1102×860200–450
KTE-65D62.4300–800132–1602×1530350–600
KTE-75B71500–600132–1602×1530300–800
KTE-75D71300–800200–3152×2100500–1000
KTE-85B85500–600220–3152×2100550–1000
KTE-95B93500–600250–3152×3000800–1500
KTE-95D93500–800315–5002×48001000–2000
KTE-135B135500–600315–5002×48001500–3000
KTE-135D135500–800500–10002×78001500–4000

Tiga kesalahan paling mahal

1. Memberi feed serat ke hopper utama merusak panjang serat dan disperse.

Memberi feed serat ke hopper utama merusak panjang serat dan disperse.

2. Elemen sekrup baja standar aus dalam beberapa bulan pada 40% GF.

Elemen sekrup baja standar aus dalam beberapa bulan pada 40% GF.

3. Menentukan ukuran hanya dari kg/h

Menentukan ukuran hanya dari kg/h — tugas serat kaca dibatasi torsi; gearbox yang dipertahankan di atas 85% torsi di setiap shift membuat oli overheat dan memotong umurnya menjadi setengah.

FAQ

Panjang serat berapa yang dipertahankan?

0.4–0.7 mm di dalam pellet untuk grade GF standar; serat panjang (>10 mm) membutuhkan lini LFT terpisah.

Satu mesin bisa menjalankan GF dan filler mineral?

Bisa dengan pergantian set sekrup dan rutinitas pembersihan yang benar; residu GF mengkontaminasi batch berfiller mineral secara kasatmata.

Output berapa yang bisa kalian jamin untuk aplikasi ini?

Band referensinya adalah 300–2,500 kg/h, diukur pada material yang dinyatakan. Kami menawarkan angka terjamin hanya setelah uji coba pada material Anda sendiri, karena grade filler, bulk density, dan kelembapan menggeser output ±15%.

Bisakah kami menjalankan material kami sebelum memesan?

Ya — untuk lini compounding serat kaca, kirim 25–50 kg compound-nya; laporannya menambahkan panjang serat residu dan riwayat suhu lelehan. Anda juga menerima pellet, video berjalan, serta suhu, kecepatan sekrup, dan setelan feeder yang kami pakai. Uji cobanya gratis; Anda menanggung fretenya.

Berapa waktu pengirimannya?

30–45 hari kerja untuk konfigurasi standar lini compounding serat kaca, 45–70 untuk geometri sekrup kustom dan pekerjaan ODM — side feeder dan melt pump ditawarkan bersama lininya. Tegangan dan frekuensi dibangun untuk negara tujuan.

Dari mana angka-angka ini berasal

Parameter di halaman ini (lini compounding serat kaca) diambil dari tabel parameter produk Kerke dan lembar data induk produk, serta disilangkan dengan rekaman commissioning lini compounding yang dibangun dalam beberapa musim terakhir. Formulasi dan jendela suhu adalah nilai tipikal industri untuk paduan rekayasa dan serat, bukan rekomendasi untuk compound spesifik Anda — setiap angka yang ditandai referensi harus dikonfirmasi lewat uji material sebelum menjadi angka kontraktual.

Direview oleh tim proses Kerke, Nanjing. Halaman diperbarui 6 November 2026.

Katakan material Anda — kami sebutkan lininya

Kirim 25–50 kg untuk uji coba lini compounding serat kaca pada extruder laboratorium kami: pellet, video berjalan, dan laporan kapasitas kembali dalam 3–7 hari — laporannya menyertakan panjang serat residu di samping kapasitas.

Compounding serat kaca — versi singkat

Catatan tentang compounding serat kaca: angka-angka di atas adalah rentang referensi dari uji coba kami sendiri di Kerke, bukan janji katalog. Geometri sekrup, paket anti-usang, dan metode pelletizing ditentukan lebih dulu di bangku uji, jadi output yang Anda bandingkan adalah output yang Anda dapatkan. Jika grade Anda tidak ada di tabel, kirimkan — konfigurasi terdekat biasanya berupa pergantian set sekrup, bukan mesin yang berbeda.

Terkait di situs ini: Machine range: KTE-50B to 135D · Pelletizing methods compared · penawaran dan uji coba gratis · Wikipedia: Masterbatch